000126 Spring Green Opalescent

Spring Green Opal, 000126-0030-F

Overview

Striker

This style may not reveal (strike to) its target color until fired.

Reactive Potential

Contains: Sulfur (S) / Selenium (Se)
May React With: Copper (Cu), Lead (Pb), and Silver (Ag)

Forms of Glass

Sheet Glass (-0030, -0050), Frit (-0001, -0002, -0003, -0008), Rod (-0576), Stringer (-0507, -0107, -0272), and Ribbon (-0401)

Detailed Information

About 000126 Sheet Glass
Cold Characteristics

Color variations common from minty-pastel to vibrant yellow-green.

000126-0050-F
000126-0050, 2mm Cold Sheet
000126-0030-F
000126-0030, 3mm Cold Sheet
Working Notes

Lighter coloration matures and becomes consistent to target upon firing.

A sulfur glass. May react with lead and copper glasses to create dark interface (lead sulfide, copper sulfide).

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

Spring Green Opal, 000126-0030-F
000126-0030, Fired Tile
About 000126 Frit
Working Notes
000126-0003-F
000126-0003
Coarse Frit
000126-0002-F
000126-00032
Medium Frit
000126-0001
000126-0002
Fine Frit
000126-0008
000126-0008
Powder

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

About 000126 Rod
Cold Characteristics
000126-0576-F
000126-0576, Rod

Slight variations from one production run to another.

Working Notes

Torch: Lighter color and greater opacity than in sheet glass form. Keep it a bright chartreuse by working with a neutral to oxidizing flame atmosphere. Can turn gray in reduction.

Kiln: Lighter color and greater opacity than in sheet glass form.

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

About 000126 Stringer
Working Notes
000126-0272-F
000126-0272, 2mm Stringer
000126-0107-F
000126-0107, 1mm Stringer
000126-0507-F
000126-0507, .5mm Stringer

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.

About 000126 Ribbon
Working Notes
000126-0401-F
000126-0401, Ribbon

This style is not suitable for kilncasting because it can become incompatible when held at high temperatures for an extended period. It may also become incompatible in instances where processes exceed the parameters of the test for compatibility. Testing recommended when heatwork exceeds these parameters.